electromagnetic separator dry type
Séparateur Électromagnétique (Type Sec)
Industrial Wet-Type Electromagnetic Separator for Battery Slurry Purification
Séparateur Électromagnétique (Type Humide)
eddy currrent separator
Combinaison d'un séparateur à courants de Foucault excentrique et d'un séparateur d'acier inoxydable
Électro-aimant autonettoyant
Filtre magnétique automatique pour poudre
Séparateur Magnétique à Bande Transporteuse
Piège magnétique automatique pour liquides
Séparateur Magnétique Rotatif Automatique à Grille
Séparateur Magnétique Rotatif Automatique à Grille
Minerals & kaolin

Magnetic Separation for Kaolin and Mineral Processing

Wet high-intensity separation for weakly magnetic iron- and titanium-bearing minerals where brightness, whiteness and grade define acceptance.

Kaolin slurryWeak magneticsBrightnessHigh intensity
Review equipment options
Wet high intensity magnetic separator for kaolin purification
Application image for this industry page.
23,000 GsHigh-intensity field
WetSlurry circuit
Fe / TiTarget minerals

Aperçu

Kaolin brightness and grade are limited by iron- and titanium-bearing minerals that arrive with the ore and survive conventional processing. Much of that contamination is only weakly magnetic, so a standard grate or drum will pass it. Removing it requires a high-intensity field applied to a dispersed slurry, which is why kaolin brightening is a wet high-intensity duty rather than a tramp-metal duty. The same principle applies across mineral processing — feldspar, silica sand, calcium carbonate and ceramic raw materials all face a similar weakly magnetic fraction. A wet high intensity magnetic separator is the equipment this duty requires.This page covers what limits brightness, why intensity matters, how the circuit is arranged, and what to specify.

Kaolin slurry purification with a high-gradient magnetic matrix
Application view

A coarse stage protects the high-intensity matrix

Kaolin, feldspar, silica and ceramic raw materials require a circuit built around mineralogy, dispersion, residence time and matrix cleaning.

What Limits Kaolin Brightness and Grade

Brightness is a measure of how much light the powder reflects, and iron-bearing minerals absorb light rather than reflect it. Even a small fraction changes the measured value, which is why brightness specifications are tight and why contamination that would be invisible in a bulk chemical matters here.

The minerals responsible fall into two groups. Discrete iron oxide and hydroxide particles — hematite and goethite among them — are the more straightforward case, because they are separate particles that can be captured if the field is strong enough. Titanium-bearing minerals such as anatase, rutile and ilmenite are the harder case: some occur as liberated particles, but some are associated with the clay structure itself, where no mechanical separation can reach them.

That distinction sets the realistic expectation for magnetic separation. It removes liberated magnetic and weakly magnetic particles effectively. It does not remove iron or titanium that is structurally part of the clay particle. A circuit that is expected to solve both will under-deliver, and the shortfall is usually attributed to the equipment rather than to the mineralogy.

Particle size adds a second constraint. Kaolin is processed fine, and the fines carry a disproportionate share of the contaminating minerals. A separator that works on the coarse fraction will report good recovery while the product brightness stays flat.

Why Weakly Magnetic Minerals Need High-Intensity Separation

Field strength alone is not the variable that matters. Capture depends on the field gradient at the matrix surface, the residence time in the field, and the magnetic susceptibility of the particle.

Iron-bearing minerals in kaolin have low susceptibility compared with ferrous metal. A standard ferrite or neodymium element produces a gradient that is adequate for tramp metal and inadequate for these minerals. The particle passes through the field without being captured, and the test reports the expected removal of coarse iron with no change in brightness.

High-intensity electromagnetic separation addresses this by combining a strong background field with a matrix that concentrates the gradient. The trade-off is that the matrix is fragile in the wrong hands: it blinds if coarse material reaches it, and it needs a flush cycle to release what it has captured. Both of these shape the circuit design rather than being operating details.

The practical consequence is that a high-intensity stage is always preceded by a coarse stage. Placing the high-intensity element directly after the blunger or screen means it spends its capacity on material the coarse stage should have removed.

The Wet High-Intensity Circuit in Practice

Kaolin is treated as a dispersed slurry, so the circuit is built around slurry handling rather than around a single unit.

Dispersion and screening. The clay is blunged and screened to remove coarse material and oversize. This protects the matrix downstream and stabilises the feed.

Coarse magnetic removal. A drum or grate stage removes the ferrous fraction that would otherwise blind the high-intensity matrix. This stage is cheap and protects an expensive one.

High-intensity separation. The slurry passes through the matrix in the background field. Residence time, solids loading and field setting determine recovery. A wet type electromagnetic separator is the unit used at this position, sized on slurry flow rather than on dry throughput.

Flush and matrix cleaning. Captured material is released on a cycle. If the flush is incomplete, the matrix progressively blinds and recovery falls without any change in the field reading.

Dewatering and product handling. Downstream of separation, the slurry is dewatered and dried. Contamination introduced here — from unlined equipment or from wear — is not recoverable by the separator upstream.

For coarser mineral streams where the magnetic fraction is more strongly responsive, a drum type magnetic separator covers the duty at higher throughput and lower intensity. The choice between drum and high-intensity matrix follows the susceptibility of the target mineral, not the tonnage.

Wet High Intensity Magnetic Separator Equipment for Kaolin

Kaolin circuits combine a coarse protection stage with a high-intensity stage, and the units below cover both positions. Each links to the product page with its field rating and construction details; the working figure is confirmed against the actual feed at quotation stage.

ÉquipementFieldPosition it serves
Wet type electromagnetic separator23,000 GsHigh-intensity stage on dispersed kaolin slurry
Vertical ring high gradient separatorHigh-gradient, oil-water cooledContinuous high-intensity duty at larger throughput
Drum magnetic separator8,000 GsCoarse ferrous removal ahead of the high-intensity stage
Séparateur à tambour magnétique demi-cercleUp to 6,000 GsDry bulk and powder streams
Magnetic pulley separator15,000 GsConveyor head pulley, continuous tramp removal
Cross belt magnetsPermanentOverhead conveyor duty with self-cleaning
Self-cleaning hump magnet12 000 GAbrasive bulk material in gravity chutes
Conveyor belt magnetic separator15,000 Gs dual-stageConveyor lines requiring two-stage removal
Magnetic bar and tube separator14 000 GsPipe transfer and silo outlets

The pairing is the design decision, not the individual unit. A high-intensity matrix is the most expensive element in the circuit and the easiest to damage, so the coarse stage ahead of it is what determines whether the high-intensity stage survives its first month. Where the feed varies with the ore body, sizing the coarse stage for the worst case rather than the average is the cheaper choice over a season.

Selection Inputs for Kaolin

Kaolin circuits are specified on slurry behaviour and mineralogy, not on tonnage alone.

  • Target brightness and grade — the specification that has to be met, expressed in the same units the lab reports.
  • Mineralogy of the contaminant — which iron and titanium minerals are present, and how much is liberated rather than associated with the clay.
  • Feed particle size distribution — the fines fraction usually carries the contamination.
  • Solids loading — sets viscosity and therefore residence time in the matrix.
  • Slurry flow rate — the sizing basis for a wet high-intensity unit.
  • pH and dispersion state — affects whether particles report as discrete entities or as flocs.
  • Flush water availability and quality — the flush cycle is part of the process, not an afterthought.
  • Matrix and housing material — abrasion from the slurry determines wear life.

The most common specification error is quoting a unit on dry tonnage. A wet circuit is sized on slurry volume and residence time, and two plants with the same tonnage but different solids loading need different equipment.

How It Compares With Chemical Bleaching

Magnetic separation and chemical bleaching are usually presented as alternatives. In practice they address different fractions, and most brightening circuits use both.

Séparation magnétiqueReductive bleaching
TargetLiberated magnetic and weakly magnetic particlesDissolved and surface iron
MechanismPhysical capture in a fieldChemical reduction to a soluble form
Effect on titanium mineralsRemoves liberated titanium-bearing particlesLimité
Reagent and effluentAucunReducing agent and effluent handling
Operating cost profileMainly power and maintenanceMainly reagents
Position in the circuitBefore bleaching, to reduce the loadAfter separation

The ordering matters. Removing the liberated magnetic fraction first reduces the reagent demand of the bleaching step and reduces the solids that would otherwise consume reagent. A circuit that bleaches without prior magnetic removal carries a reagent cost that the separation step would have avoided.

For ceramic raw materials where the contamination profile is similar, the approach and the quality measures are set out in enhancing ceramic purity.

Quality Control and Verification

Brightness is measured on the product, but it is a lagging indicator — by the time it moves, the circuit has been off for a while. Two leading indicators are more useful.

The first is the field and matrix condition. Field measurement on each element against the unit serial number confirms the unit is as specified; the flush cycle record confirms the matrix is being cleaned. Together they explain most of the drift that appears as a brightness change.

The second is a periodic spiked-slurry test at the operating velocity. This gives a recovery figure for the actual feed, which is the only number that predicts performance when the ore body changes. The method is described in the processus d'essai du séparateur magnétique.

When the ore source changes, re-run the test rather than adjusting the field setting by feel. A change in mineralogy alters which fraction is responsive, and the correct response is often a change in residence time rather than in intensity.

To have a kaolin or mineral circuit reviewed against a specific feed and brightness target, send the material data through the customisation enquiry.

Foire aux questions

Can magnetic separation replace chemical bleaching entirely?
Usually not. Magnetic separation removes liberated magnetic particles; bleaching addresses dissolved and surface iron that no physical field can capture. Where the contamination is predominantly liberated particles, the magnetic stage does most of the work, but the residual dissolved fraction still needs a chemical step.
Why does the brightness not improve after installing a separator?
The most common reasons are that the contaminating minerals are associated with the clay structure rather than liberated, that the matrix is blinding because the coarse stage is missing, or that the flush cycle is incomplete. Mineralogy is the first thing to check, not field strength.
Does a stronger field always give better recovery?
No. Below a certain particle susceptibility no practical field will capture the particle, and above a certain residence time additional intensity adds cost without recovery. Residence time and dispersion usually offer more improvement than a higher field setting.
How is performance verified on a production circuit?
By a spiked-slurry test at the operating velocity, combined with field measurement on each element and a flush-cycle record. Product brightness alone is too slow to catch a developing problem.
Engineering review

Match the field, housing and cleaning method to the actual stream.

Send the material form, particle size, throughput, temperature, line pressure and target contamination level for a configuration review.